Hi We have a new product that has a 22uF 0805 X5R 6.3V Ch... - Apr 26, 2006 by
Hi Darren, First thing is to check the footprint against ... - Apr 26, 2006 by Rob
Since the connection improves when you touch it with a solde... - Apr 26, 2006 by davef
I've seen failures like this with multilayer parts that seem... - Apr 26, 2006 by
I'm guessing it's part No. GRM21BR60J226ME39, which has a Ma... - Apr 26, 2006 by Rob
I find is fascinating that a lot of people blame the Pbfree ... - Apr 26, 2006 by muse
Most of Murata's parts were changed over by 1996, except hig... - Apr 27, 2006 by Rob
Darren