Hello, I have recived from customer PCB where he found th... - May 17, 2006 by
What color is the pad? coated with solder?, black?, still go... - May 17, 2006 by RDR
Hi , It looks like there is solder (shiny like mirror surfa... - May 17, 2006 by
I would suspect touch-up/repair, unless all your caps are fa... - May 17, 2006 by
Chunks learn to spell first, then you can place blame on the... - May 17, 2006 by Dr Shocker
Good post WML! you helped a lot!, Chunks brings up good ... - May 18, 2006 by RDR
Perhaps a PhD should be able to recognize the difference bet... - May 18, 2006 by Steve Thomas
Are you seeing added solder or is it possible you're looking... - May 18, 2006 by Steve Thomas
Thanks Doctor - as always, you're right. I must've been typ... - May 18, 2006 by
Hi Mark, I feel like a broken record since I keep replyin... - May 18, 2006 by
Hypothesis #1: We agree with Steve. You are probably seein... - May 18, 2006 by davef
Mark