I have been getting non wets on fine pitch QFP packages on r... - Sep 07, 2006 by Vick
Check for coplaner leads if this just exists at reflow proce... - Sep 07, 2006 by
Did check the coplanarity of the failed lead and found it to... - Sep 07, 2006 by Vick
OK, part touching paste before reflow? Check part. Maybe b... - Sep 07, 2006 by
Is the solder reflowing on the pad but not wicking up the le... - Sep 07, 2006 by Steve Thomas
Can u elaborate on the bad plating? Have u had any experienc... - Sep 07, 2006 by Vick
Yes solder is reflowing on the pad but doesnt wick up the le... - Sep 07, 2006 by Vick
Questions are: * So after you spot one of these leads sitti... - Sep 07, 2006 by davef
Yes the part is reworked. It solders when it's reworked. ... - Sep 07, 2006 by Vick
That's your clue. Your reflow is running ~240*C and your so... - Sep 08, 2006 by davef
By profile (profile has not been changed) are you referring ... - Sep 08, 2006 by Steve Thomas