We are currently experiencing some MCSB's on 0603 components... - Sep 22, 2006 by Dback
Be careful of inverted homeplates if you hand clean your ste... - Sep 22, 2006 by Real Chunks
For this inverted homeplate, the edges are rounded vs. spike... - Sep 25, 2006 by Dback
Yup, seen them too. Be care not to apply too much squeegee ... - Sep 25, 2006 by Real Chunks
We are just getting into full production on a handful of lea... - Sep 25, 2006 by
Thnaks for the tips so far. I am currently reading our paste... - Sep 25, 2006 by Dback
Have you tried an alternative paste supplier. I have ran ... - Sep 26, 2006 by
me and my big mouth. we are currently running a leadfree ... - Sep 26, 2006 by
Just to update you on what I have found. I was using Indi... - Sep 26, 2006 by
We have solved our MCSB problems by using standard homeplate... - Sep 26, 2006 by Steve