Printed Circuit Board Assembly & PCB Design Forum
SMT electronics assembly manufacturing forum.
Views: 8755
Hi All, I would like to get some inputs regarding this.... ... - Aug 21, 2007 by OP3799
Questions are: * Do these pads take solder? How well? * H... - Aug 22, 2007 by davef
Hi, in past we had an issue with ENIG surface, black was Ni... - Aug 23, 2007 by d0min0
Hi Davef, Thanks for the reply. There seem to be no issues... - Aug 26, 2007 by OP3799
Actually, you will be soldering and wire bonding to the pall... - Aug 27, 2007 by davef
EDS @ 10kV maybe going too deep. I've talked to a surface s... - Aug 30, 2007 by blnorman