I am trying to optimize my reflow profile. i have a 5 zone o...
- Jul 25, 2008
by
brettc
What paste are using? You should referance the manufactures ...
- Jul 25, 2008
by
Chip_Flip
I am not very concerned about production time, but it is alw...
- Jul 26, 2008
by
brettc
Ideal situation is get a technical rep from the solder paste...
- Jul 28, 2008
by
blnorman
Do you have a Slim-Kic? You can run a profile and then do p...
- Jul 28, 2008
by
Real Chunks
thanks, looks like an interesting product. any idea of the c...
- Jul 28, 2008
by
brettc
Take a look at this. Remember, these are only guidlines and...
- Jul 28, 2008
by
garyr
my oven has a built in profiler, it works fairly well, but i...
- Jul 28, 2008
by
brettc
Oh, well if you can profile, model your profile to the profi...
- Jul 29, 2008
by
Real Chunks
Some profiles can be difficult to get exactly, so I was wond...
- Jul 29, 2008
by
brettc
Slight variations should have little impact on your product ...
- Jul 29, 2008
by
Real Chunks
You can keep only the 5th zone as the reflow zone. And lower...
- Aug 01, 2008
by
Leo
Is there a limit to the time that most components can stay a...
- Aug 02, 2008
by
brettc
If you have concerns, you can look at the datasheet for each...
- Aug 04, 2008
by
garyr
brettc