dirty wave soldering machine

Views: 1874

#56132

dirty wave soldering machine | 23 August, 2008

Hi! Does any one can give the reason of the black dust into de wave solder machine. We can found no reason for that, but the machine get dirty to fast despite the maintenance. Thanks for your time Bruna Neto

reply »

#56138

dirty wave soldering machine | 25 August, 2008

That's just dross. If you have nitrogen blowing over the wave, you could reduce its flow as it tends to blow the dust everywhere if it is set too high. (on the other hand it might reduce solder quality)

reply »

#56216

dirty wave soldering machine | 27 August, 2008

hi loco,

Thanks for your post, it was very helpfull.

reply »