Printed Circuit Board Assembly & PCB Design Forum
SMT electronics assembly manufacturing forum.
Views: 4853
I have a VJE Summit 750 Rework machine... I don't think tha... - Apr 03, 2009 by Ed Faranda
Cause: Solder between the pad and the BGA on the pads being ... - Apr 04, 2009 by davef
I agree the longer soak will help provided you are not apply... - Apr 06, 2009 by C111
Here are some pictures of the part. I created a profile ... - Apr 06, 2009 by Ed Faranda
I would use almost the same profile you use when putting the... - Apr 08, 2009 by Steve
Another suggestion for it. Baking the whole boards before re... - Apr 09, 2009 by fowlerchang
Well, I did manage to solve this problem. I lowered the max... - Apr 09, 2009 by Ed Faranda