Printed Circuit Board Assembly & PCB Design Forum
SMT electronics assembly manufacturing forum.
Views: 22452
HI Please Advice witch material can stand more heat FR4 or... - May 25, 2010 by Fotis
Hi fotis, Big difference between Cem3 & FR4 is that FR4 t... - Jun 04, 2010 by BoardHouse
Thanks My mistake on the previous post is that the Tempe... - Jun 04, 2010 by Fotis
At 400C, I'd worry about the solder as well.... ... - Jun 04, 2010 by MikeS
So..? FR4 or CEM3 ? ... - Jun 15, 2010 by Fotis
I would be concerned with either material at that temp. ... - Jun 16, 2010 by BoardHouse
You should do some testing what temp you really get. Solder ... - Jun 22, 2010 by leadthree
welcome to PCB Partner, there are more than 2300 PCB supplie... - Jun 23, 2010 by pcbpartner