We are having a problem with inspection markings on our boar...
- Jul 02, 2012
by
mccabekev
It'll probably help to know what type of coating you're usin...
- Jul 02, 2012
by
dontfeedphils
We are applying a SR conformal coating via aerosol.
Both ...
- Jul 02, 2012
by
mccabekev
Unfortunately our customers expect this coating on the board...
- Jul 03, 2012
by
mccabekev
Unfortunately our customers expect this coating on the board...
- Jul 03, 2012
by
mccabekev
Check with the coating manufacturer and see if they can offe...
- Jul 03, 2012
by
blnorman
Try this:
...
- Jul 03, 2012
by
Don Cattoni
What is the specific make/model of the SR? Being in an aeros...
- Jul 05, 2012
by
Lou
I have found that Edding do an aerospace marker, which is wa...
- Jul 16, 2012
by
mccabekev
We use the Edding pen as stated but then apply a quick set e...
- Jul 18, 2012
by
leeg
How are you applying the expoxy resin?
Why use the expens...
- Jul 18, 2012
by
mccabekev
mccabekev,
How are you applying the mark? Can you scribe...
- Jul 23, 2012
by
Reese