Dear all, can we use metal screw driver for mixing of solder paste.what are the disadvantages. please tell me.

reply »

#69835

solder paste mixing manually | 16 July, 2013

The screwdriver can scrape pieces of the plastic jar off and contaminate the paste if you aren't careful.

reply »

#69836

solder paste mixing manually | 16 July, 2013

Just pick up some of the plastic putty knifes, pretty cheap.

reply »

#69848

solder paste mixing manually | 16 July, 2013

Dear Sir,

Thank you very much for your suggestion.

reply »

#69849

solder paste mixing manually | 17 July, 2013

Dear Sir,

Thank you very much for your suggestion.

reply »

SMT Reflow Soldering Equipment Company of the Year 2020!

Online IPC Training & Certification