We had a solder joint problem in gold plated PLCC68 ic. We ... - Jul 26, 2013 by anilw2006
If there is a way to pre-tin the parts, that might help in f... - Jul 26, 2013 by Evtimov
Thanks for support. Is it any special process of pre-tinng?... - Jul 29, 2013 by anilw2006