My company is researching the use of re-workable underfill f... - Mar 27, 2014 by Rob R.
If you are 100% sure that the solder has reflowed (time and ... - Mar 27, 2014 by Hegemon
hege: beer can opener!!! The ultimate multipurpose tool ... ... - Mar 28, 2014 by davef
With heat, most underfills soften just before the solder mel... - Mar 28, 2014 by davef
Lol Dave. Give me a lever long enough.... ... - Mar 28, 2014 by Hegemon
Hi, sorry for reopening a old thread, but i wanted to ask if... - Sep 28, 2015 by Dacian B.
The melting point of the solder itself does not change when ... - Sep 28, 2015 by dyoungquist