i HAVE A CUSTOMER WHO IS USING A WATER SOLUBLE LEAD FREE SOL... - Oct 05, 2018 by Steve
Paste sticking to squeegee: * Squeegee is heavily magneti... - Oct 05, 2018 by davef
The stuff Dave mentioned are the fundamentals. If the items ... - Oct 08, 2018 by Sr. Tech
+paste was not stored properly Paste doesn't have enough fl... - Oct 08, 2018 by Evtimov
This problem frequently becomes an issue with lead free sold... - Oct 10, 2018 by Netvicher123
I do not agree with that. Stainless is typically used a... - Oct 10, 2018 by Sr. Tech
davef The rest of your list looks good, but I'm not buyin... - Oct 10, 2018 by dwl
This is an old joke of Dave's... ... - Dec 13, 2018 by Tom
Gotcha. Apparently I'm gullible... ... - Dec 13, 2018 by dwl
High quality coated blades are easier to clean but has zero ... - Dec 14, 2018 by Jandon