Hello all, I have a crystal that breaks in spinning test ... - Nov 28, 2018 by Evtimov
I think silicone mask is ok, This is so that after soldering... - Nov 29, 2018 by Cannizzaro
is it vibration or pcb bends under G force? what angle is th... - Nov 29, 2018 by bukas
You may want to look at a product called place & bond underf... - Nov 29, 2018 by Robl
Robl, I like this underfilm. Do you think you should plac... - Nov 29, 2018 by Evtimov
Hi Evtimov, For BGA's you place 4 on each side right outs... - Nov 29, 2018 by Robl
Thanks Rob, in my case I will probably have it in the mid... - Nov 29, 2018 by Evtimov
Thanks,@Robl for sharing. ... - Jan 08, 2019 by Mermar
Hi Mermar, you're welcome. ... - Jan 08, 2019 by Robl