Printed Circuit Board Assembly & PCB Design Forum
SMT electronics assembly manufacturing forum.
Views: 697
We are using Wertheim SMT Reflow oven.We are facing componen... - Aug 13, 2019 by Sankar
Too much heating on the bottom side surely? ... - Aug 13, 2019 by Spoiltforchoice
It Satisfy Profile Condition ... - Aug 13, 2019 by Sankar
A profiler can't distinguish where your heat is coming from,... - Aug 13, 2019 by Steve Thomas
To be in the range of profile for a paste, doesn't mean it i... - Aug 16, 2019 by Evtimov
It is quite of great information, I'm glad to visit this use... - Aug 17, 2019 by promoocodes