Quad qsv1 plus | 20 January, 2020

Hi, my company bough second hand pick and place as our second machine. After first transport after start just when initializing, It's showing problem with Z calibration. After second position setup and connect again after month, now showing "door interlock open" even doors is closed and whole cables is not loose-was checked about connection. Anybody got similar problems?

Attachments:

reply »

#84234

Quad qsv1 plus | 20 January, 2020

Hello, You have a tep initialize issue. Please contact me. If you need my email go to my website and i would be glad to help.