DEK PRO-FLOW installation | 9 February, 2021

I have a DEK Horizon 02i. Is it easy to swap between Squeegee and cartridge system just by installing the Proflow head assembly?

reply »

#86253

DEK PRO-FLOW installation | 9 February, 2021

Unfortunately, with the Micron ('i') series of machines, DEK seemed to stop making "ProFlow Ready" the standard on machines. In general, there are additional pneumatics and electronics required for a ProFlow installation.

reply »

#86254

DEK PRO-FLOW installation | 9 February, 2021

Thanks, we have an 03i. Whats the difference between 02i and 03i?