Need suggestions on conformal coat curing oven | 13 April, 1999

I need to cure conformal coat on a 19" x 15" board. The material needs 7 - 10 minutes at 100deg C, but I have limited floorspace so I'm looking for an oven with about 36 inches heated length and 18 or more inch wide belt. The material we are considering is a solventless 2 part polyurethane. No VOC emissions is a big factor in the material choice. We are an OEM, so I have some leeway in material choice if anyone has a suggestion. Thanks, Mike.

reply »

Stephen Oltmann

#11966

Re: Need suggestions on conformal coat curing oven | 14 April, 1999

| I need to cure conformal coat on a 19" x 15" board. The material needs 7 - 10 minutes at 100deg C, but I have limited floorspace so I'm looking for an oven with about 36 inches heated length and 18 or more inch wide belt. The material we are considering is a solventless 2 part polyurethane. No VOC emissions is a big factor in the material choice. We are an OEM, so I have some leeway in material choice if anyone has a suggestion. | Thanks, Mike. |

reply »

Stephen Oltmann

#11967

Re: Need suggestions on conformal coat curing oven | 14 April, 1999

Check with BTU. They have dryers in the length you need.

Good luck!

| | I need to cure conformal coat on a 19" x 15" board. The material needs 7 - 10 minutes at 100deg C, but I have limited floorspace so I'm looking for an oven with about 36 inches heated length and 18 or more inch wide belt. The material we are considering is a solventless 2 part polyurethane. No VOC emissions is a big factor in the material choice. We are an OEM, so I have some leeway in material choice if anyone has a suggestion. | | Thanks, Mike. | | | |

reply »

#11968

Re: Need suggestions on conformal coat curing oven | 14 April, 1999

| I need to cure conformal coat on a 19" x 15" board. The material needs 7 - 10 minutes at 100deg C, but I have limited floorspace so I'm looking for an oven with about 36 inches heated length and 18 or more inch wide belt. The material we are considering is a solventless 2 part polyurethane. No VOC emissions is a big factor in the material choice. We are an OEM, so I have some leeway in material choice if anyone has a suggestion. | Thanks, Mike. | Mike: Bag the conveyorized oven thing. It'll be too big and too slow. Buy a used Blue M oven from LR Environmental. TTYL Dave F

reply »

Graham Naisbitt

#11969

Re: Need suggestions on conformal coat curing oven | 17 April, 1999

Mike

First, you MUST make sure the oven used is extracted.

The coating will contain TDI. This is not nice.

You would be better considering a silicone solventless. Try contacting HumiSeal. They had a material on the TAC line at Nepcon West that looked good 1C61 I think.

Hope this helps and is not too late. Let me know if you want more. | I need to cure conformal coat on a 19" x 15" board. The material needs 7 - 10 minutes at 100deg C, but I have limited floorspace so I'm looking for an oven with about 36 inches heated length and 18 or more inch wide belt. The material we are considering is a solventless 2 part polyurethane. No VOC emissions is a big factor in the material choice. We are an OEM, so I have some leeway in material choice if anyone has a suggestion. | Thanks, Mike. |