Need to automatically dispense latex masking material | 9 November, 1998

I have a need to dispense a latex masking material using an automated dispensing system. We are presently looking at the I&J750. Does anyone have any experience with this piece of equipment, or have a better solution available?

reply »

Dave F

#13555

Re: Need to automatically dispense latex masking material | 10 November, 1998

| I have a need to dispense a latex masking material using an automated dispensing system. We are presently looking at the I&J750. Does anyone have any experience with this piece of equipment, or have a better solution available? | Doug: Fisnar makes a good low end disponser. Have you considered printing your latex solder mask? Dave F

reply »

Wayne Bracy

#13556

Re: Need to automatically dispense latex masking material | 11 November, 1998

| I have a need to dispense a latex masking material using an automated dispensing system. We are presently looking at the I&J750. Does anyone have any experience with this piece of equipment, or have a better solution available? |

Doug:

You might want to take a look at Specialty Coating Systems. I have attached their URL so you can go and look at their website. They manufacture conformal coating equipment really nice stuff and good people to work with.

Wayne

reply »

Doug Clement

#13557

Re: Need to automatically dispense latex masking material | 12 November, 1998

| | I have a need to dispense a latex masking material using an automated dispensing system. We are presently looking at the I&J750. Does anyone have any experience with this piece of equipment, or have a better solution available? | | | Doug: Fisnar makes a good low end disponser. Have you considered printing your latex solder mask? Dave F | Dave, I am unable to print. We are looking at the Fisnar I&J750. Have you used the I&J500 or 750? If so, what problems have you had?

reply »

Dave F

#13558

Re: Need to automatically dispense latex masking material | 12 November, 1998

| | | I have a need to dispense a latex masking material using an automated dispensing system. We are presently looking at the I&J750. Does anyone have any experience with this piece of equipment, or have a better solution available? | | | | | Doug: Fisnar makes a good low end disponser. Have you considered printing your latex solder mask? Dave F | | | Dave, I am unable to print. We are looking at the Fisnar I&J750. Have you used the I&J500 or 750? If so, what problems have you had? | | Doug: We looked at:

TechnoISEL, 2101 Jericho Turnpike, NHyde Park, NY 11040 516.328.3970 fax 8827 ($14k) Online 815.363.8008 (RC1818 $17k) DCI, One Kenwood Circle, Franklin MA 02038-9908 800.341.4811 fax 508.520.1424 $10k IJ Fisnar ($10k) 201.796.1477 fax 794.7034 Manncorp Box8 1840 Country Line Rd Unit 101 Huntington Valley PA 19006 800.745.6266 215.364.6100 fax 6110 www.manncorp-smt.com

We selected Manncorp because we liked the idea of using Gerber data, rather than visually locating, the placement head. Not that that's a big deal, when slopping latex on a board. Generally, we were disappointed in the "programming interface," what ever that is, with all machines. These are, from a programming stand-point, fairly crude activities. We were hoping to have this be operator programmable, without a lot a two letter secret codes. You know click on "go right," rather than press "MOV/9" twice.

On Fisnar, we wanted to be able to do a 16" square board, they couldn't do that.

TTYL

Dave F

reply »

Doug Clement

#13559

Re: Need to automatically dispense latex masking material | 13 November, 1998

| | | | I have a need to dispense a latex masking material using an automated dispensing system. We are presently looking at the I&J750. Does anyone have any experience with this piece of equipment, or have a better solution available? | | | | | | | Doug: Fisnar makes a good low end disponser. Have you considered printing your latex solder mask? Dave F | | | | | Dave, I am unable to print. We are looking at the Fisnar I&J750. Have you used the I&J500 or 750? If so, what problems have you had? | | | | | Doug: We looked at: | | TechnoISEL, 2101 Jericho Turnpike, NHyde Park, NY 11040 516.328.3970 fax 8827 ($14k) | Online 815.363.8008 (RC1818 $17k) | DCI, One Kenwood Circle, Franklin MA 02038-9908 800.341.4811 fax 508.520.1424 $10k | IJ Fisnar ($10k) 201.796.1477 fax 794.7034 | Manncorp Box8 1840 Country Line Rd Unit 101 Huntington Valley PA 19006 800.745.6266 215.364.6100 fax 6110 www.manncorp-smt.com | | We selected Manncorp because we liked the idea of using Gerber data, rather than visually locating, the placement head. Not that that's a big deal, when slopping latex on a board. | Generally, we were disappointed in the "programming interface," what ever that is, with all machines. These are, from a programming stand-point, fairly crude activities. We were hoping to have this be operator programmable, without a lot a two letter secret codes. You know click on "go right," rather than press "MOV/9" twice. | Dave, Thanks for the valuable information. This certainly will help us in resolving our problem.

| On Fisnar, we wanted to be able to do a 16" square board, they couldn't do that. | | TTYL | | Dave F |