Howard C. Ohlhous

#2714

Surface Mount Component Glues | 16 October, 2000

I would like to know what type of glue is used to hold down surface mount devices to boards before/during solder reflow. I would like to obtain said glue for evaluation and possible use in an assembly procedure. Please Advise: What company manufactures/distibutes said glue? Thank you Howard C. Ohlhous

reply »

#2715

Re: Surface Mount Component Glues | 16 October, 2000

Review the SMTnet archives as a good starting point for your search

reply »

#2716

Re: Surface Mount Component Glues | 17 October, 2000

Try "Amicon D125 F". Good for both dispensing and screen printing. I like the yellow colour, it shows up better on green pcbs. Most smd adhesives are single part, heat cured epoxies, UV curing having gone out of fashion some years ago. Amicon used to be distributed by "GRACE", possibly now by "Emerson & Cuming" That's my two bobs worth.

reply »

D

#2717

Re: Surface Mount Component Glues | 17 October, 2000

Try Heraeus PD955M#9

reply »