what is CEM3

reply »

Ben Bierlein

#17789

cem3 | 5 October, 2001

It is a PCB material that has a woven glass / epoxy internal core and glass veil surface. It is in between the paper materials (FR1,FR2 and CEM1) and FR-4 as far as strength and cost. It is available in HiCTI material for high power applications.