Is anyone still using Loctite 348 chipbonder for bottom side attachment? Is it truly adequate for dispensing up to 18k/hour?
We will be dispensing with a Camelot 2800, so somewhere in the neighborhood of 15k/hr. is as fast as we'll ever see.
I'm considering 3609 also as the viscosity is a little higher (according to my rep., I haven't seen the spec. sheets yet) and we'll be needing some pretty big piles in a few applications (high standoff). Is it worth the added $20/30cc's?
Another factor is the shelf life, 348 @ 9 months vs. 3609 @ 6 months. Given that our volumes will be small for two-sided assembly, this may be an issue.
Thanks all.........