Printed Circuit Board Assembly & PCB Design Forum
SMT electronics assembly manufacturing forum.
Hi, Have anyone done STSOP32 circuit with 0,5mm pitch wit... - Oct 01, 2002 by Mr.T
No, wouldn't want to, wouldn't be prudent. Best process I th... - Oct 09, 2002 by PeteC
What sorts of problems or defects are you experiencing when ... - Oct 13, 2002 by
Hi, Problem is Bridging on between leads. Br, Mr.T ... - Oct 15, 2002 by Mr.T
I can't comment on 20 pitch TSOP, but wave soldering wider p... - Oct 15, 2002 by davef
I haven't tried anything like that but had some experience w... - Oct 23, 2002 by