high temp wave soldering

aerin

#22444

high temp wave soldering | 20 November, 2002

Hi, I'm an SMT refugee working in component manufacture - hey, times are hard! I've been asked by a customer to test some of my parts at high temperature on the wave - up to 360 deg Celsius. I've checked my wave and it's only capable of getting up to 340 deg for a start! I know that if you are doing specific high temp soldering you would use a different bar with varying % of Sn and Pb. But, what would happen if we take the temp of std bar up higher? Any ideas?

reply »

#22448

high temp wave soldering | 20 November, 2002

Kester has a special alloy for high temp soldering. Alloy 123. I would think that if you coocked 63/37 to 360c you would have a pot of dross in no time!

Doug