Up until this point, my company has been hand soldering all ... - Oct 13, 2003 by
HI Andrea- to answer Q: 1) Stencils can be order through v... - Oct 13, 2003 by CAL
Hi Andrea, Another good place to start in addition to the... - Oct 13, 2003 by Larry
As far as solder paste goes search no further! I have worked... - Oct 14, 2003 by
Here is a tip. Do an evaluation on materials. DO not trust... - Oct 14, 2003 by
Hi I am going to take another direction. Go to some cl... - Oct 14, 2003 by
What works in Alaska will probably not work as well in Flori... - Oct 15, 2003 by
Why would you have troubles if and when you switch? Isn't t... - Oct 16, 2003 by
We have been unimpressed with the capability and control of ... - Oct 16, 2003 by davef
Wait a minute I thought I said Celestica and a few others ha... - Oct 17, 2003 by
Dave, Its the APS (Automated Production Systems, Inc- Hun... - Oct 17, 2003 by PeteC
Okay, I'm here in Colorado and I used indium 92J and loved i... - Oct 17, 2003 by RDR
Dave and Pete No bad words against a good batch oven. I don... - Oct 19, 2003 by harotec.ch
Who said there was NO evaluation? The paste we chose was ev... - Oct 20, 2003 by
APS themselves is a good source for learning how to use this... - Oct 20, 2003 by severs
Hey Russ I hate to say it but you switched from Indium for n... - Oct 21, 2003 by
AXL, you could be right! I personally didn't switch they di... - Oct 21, 2003 by RDR