We have had some field returns of a double sided SMT board m... - Jun 25, 2004 by
What are the specifications on the solder that you use? IE: ... - Jun 25, 2004 by Steve
We use water soluble paste, Kester R560. These units are wa... - Jun 25, 2004 by
Sounds like the wrong reflow profile was possibly used on th... - Jun 25, 2004 by RDR
We have beaten the reflow profile angle to death and haven't... - Jun 25, 2004 by
Any chance your potting compound was changed in the timefram... - Jun 25, 2004 by
The potting definitely is a factor in fracturing the grainy ... - Jun 25, 2004 by
For what its worth. Even though you are potting the boards. ... - Jun 25, 2004 by Steve
Nonductile fracture!!! Sounds peculiar. In that case, stop... - Jun 25, 2004 by davef