I'm sorry for not being clear. The "1 thou" refers to the thickness of copper that rides below your ENIG.
If your HIC card is blue that's good. If it's some other color that makes you nervous, then you make of it what you will. They're pretty much meaningless to us. We keep reusing a coffee can full of them.
Beyond that, the "card is pink" has limited value without knowing more about the storage environment, packaging, time in storage, and what not.
The shelf life of your ENIG is probably around 6 months. For pretty good comparision of various solderability protection coatings, look here: http://www.twi.co.uk/j32k/unprotected/pdfs/6feb03_aw6.pdf
[We have no relationship, nor receive benefit from the company linked above.]
Finally, on baking your boards, no one really knows, we'd just be guessing. Why no reflow a pasted [no components] board, and make an evaluation?