We agree with Paul. If you prepare the components differently, so that they snap into place, you do not need to trim after wave.
Most rotary trimmers put a HUGE amount of stress on solder connections, potentially cracking the connections.
Some of the companies that make forming equipement are: Equipment||Lead Forming||Olamef||||619.792.7328 fax 1966 ?? Equipment||Lead Forming||RotoForm||||423.266.0067 fax 0105 Equipment||Lead Forming||Streckfuss||||214.790.1614 fax 986.1148 rep Foundation Technologies Equipment||Lead Forming||TED/Heller||||818.735.5474 fax 4919 Equipment||Lead Forming||EBSOMAT||Greenwood Rd, P.O. Box 1009, Dublin, NH 03444||603-563-8108 Fax 8121 http://www.griptech.com/lead.html
Equipment||Lead Forming||Automated Production Sys||||215.938.1000 fax 8480 Equipment||Lead Forming||Hepco||||408.738.1880 fax 732.4456 Equipment||Lead Forming||General Production Devices||||970.245.0408 fax 245.9674 Equipment||Lead Forming||Manix Manufacturing||410 Pike Rd P.O. Box 1024 Huntingdon, Valley, PA 19006||215-953-9797 Fax 9399 http://www.manixmfg.com sales@manixmfg.com ||Tom LaMare John Daud Equipment||Lead Forming||Loupot: Automated Production Concept||63 Hillside Terrace Wayne N.J.07470||201.831.8300 Fax 201.633.7755||Bill Leonhardt Equipment||Lead Forming||Ebso, Industriestra�e|| 15, D-76767 Hagenbach, ||0049-07273-93580 Fax.: 0049-07273-935828 http://www.ebso.com Equipment||Lead Forming||Electro-Prep||2995 Corvin Dr Santa Clara, CA 95051-0705||408 739-6015 fax 3363 http://www.electro-prep.com
Alternately, some people use boat anchors called Contact CS400 machines to cut and clinch through hole components, prior to wave soldering.
reply »