Hi all, we are placing some of the 0306's (0603 size part... - Sep 09, 2005 by g cronin
sounds like the part is being picked up on its side....which... - Sep 09, 2005 by
If the tombstoning is thermal (occuring during reflow) then ... - Sep 09, 2005 by Rob
thanks for the feedback, The part is not on its side, it ... - Sep 09, 2005 by g cronin
Talk to your paste supplier. The reps for a couple of paste... - Sep 09, 2005 by Stephen
Try home-plated the stencil apertures, and make "V" shape ho... - Sep 09, 2005 by
thanks for the tip. Could you clarify what you mean just ... - Sep 09, 2005 by g cronin
Nomorely the V-shape home-plated apertures look like two ope... - Sep 09, 2005 by
What are the Mfg specs for pad layout? I had one that was w... - Sep 09, 2005 by RDR
If 0 or 180 degr. make v-shape openings to each other left &... - Sep 11, 2005 by
I mean we use 87 % of the original apertures. (You never kn... - Sep 11, 2005 by
hi Tombstoning can be relaited to the size of the pad, and ... - Sep 13, 2005 by