Does anybody have a slick way to hold down large inductors? ... - Feb 15, 2006 by adlsmt
Possibly a retention clip that would snap into the board? ... - Feb 15, 2006 by RDR
Bubble Yum has worked well for me in the past Brad ... - Feb 15, 2006 by Cardinal Circuit
We already tried that. The sugar seems to have a bad reactio... - Feb 16, 2006 by adlsmt
SMT adhesive? Might be able to cure in wave process? ... - Feb 16, 2006 by RDR
It is quite common for this to be done with an activator cur... - Feb 16, 2006 by davef
DaveF, would the adhesive be strong enough to keep the part ... - Feb 17, 2006 by
cmiller The materials suppliers mentioned above (eg, Dyma... - Feb 20, 2006 by davef
Can I get a sample of the Bubble Yum? Do you have several v... - Feb 22, 2006 by
try contacting emmerson and cumming they do a huge range of ... - Feb 23, 2006 by