All, I am currently trying to run a quantity of boards th... - Feb 28, 2006 by
Questions are: * What is the scale and scope of the problem... - Feb 28, 2006 by davef
Hi Davef, Basically there is very poor signs of wetting ,... - Mar 01, 2006 by
Look here: ... - Mar 01, 2006 by davef
I would definitely try a more agressive flux. Are you using... - Mar 01, 2006 by RDR
we are using a no-clean flux. ... - Mar 01, 2006 by
Outcome: More heat required... thanks to all who contr... - Mar 06, 2006 by