Hybrid flux: No-clean and WS | 12 July, 2006

Hi everybody:

I really need your expertise on this one.

I was told that the flux 270WR from AIM is either No-clean or WS soluble depending on your needs. I read the TDS and it looks like it is....but.....

Is there anybody out there using this or similar flux with those properties? I never heard of a flux like that...

I appreciate your feedback.

George

reply »


RDR

#42699

Hybrid flux: No-clean and WS | 12 July, 2006

i have heard of washable no-cleans for about 6-8 years now. I would think that if SIR values are acceptable for end use then I would run with it.

Russ

reply »

George

#42714

Hybrid flux: No-clean and WS | 13 July, 2006

Thanks Russ...