soldering thru-hole SAC305 component | 15 March, 2007

Sorry new to this...

Question: will I have any problem soldering a resistor network with SAC305 coated leads using a normal leaded wave process besides the normal board thickness issues

Thx

reply »

#48444

soldering thru-hole SAC305 component | 16 March, 2007

You should have no substantial problems soldering this component, but just in case, good luck.

reply »

#48445

soldering thru-hole SAC305 component | 16 March, 2007

SAC coated leads on certain components require more dwell time. If you find that you have top-side wetting issues, slow the conveyor down a bit or increase your wave height, or, a combination of the 2.