RF absorber

Haim B.

#7731

RF absorber | 25 January, 2000

Hello ! We are looking for a screen printable RF absorber material, to be printed on a 50 ohm line as a shielding. thanks.

reply »

#7732

Re: RF absorber | 25 January, 2000

Try:

AI Technology 70 Washington Rd Princeton Junction, NJ 08550 609) 609-799-9388 Fax: 609-799-9308 www.aitechnology.com/enter.html ait@aitechnology.com

Good luck

Dave F

reply »

Haim B.

#7733

Re: RF absorber | 26 January, 2000

Hello Mr Dave F Thanks very much. I forget to mention that the material is not electricaly cunductive.