I am going to be using a pressurized dispenser for Chemtronics CM1 peelable mask. I need to find a solvent that will work for flushing the system. I tried Xylene that we have here and it does ok, but not as good as I'd hoped. It works very well for the conformal coat sprayer, but not for the peelable mask.