PCB laminate dielectric absorption

Mike Ihm

#2209

PCB laminate dielectric absorption | 13 December, 2000

The dielectic absorption characteristic of printed circuit board materials is usually not listed on the manufacturers spec. sheets. Can anyone point me in a direction to help determine which laminate materials might exhibit better dielectric absorption characteristics than say FR-4 material.

Thanks, Mike Ihm

reply »

#2210

Re: PCB laminate dielectric absorption | 13 December, 2000

Material Dk @ 1GHz tan d @ 1GHz Difunctional 4.40 0.020 Multifunctional 4.43 0.018 Polyimide 4.06 0.006 Cyanate ester 3.65 0.005 Bismaleimide triazine 2.94 0.011 PPO-epoxy 3.85 0.012 PTFE-glass 2.60 0.001 PTFE-mat-CE 2.79 0.003 PTFE-ceramic 4.06 0.002

reply »