Re: Resistive epoxy

Kiet Dang

#11624

Re: Resistive epoxy | 29 April, 1999

Hi, Did anyone experience a problem with electrically conductive silver filled epoxy is resistive due to galvanic reaction? I'm having this problem when attaching components to Ni plated housing while conducting an experiment to cost reduction for Au plated housing. Thanks, -kiet

reply »