Solder Paste Measuring

Cuch

#12069

Solder Paste Measuring | 4 April, 1999

I need help in finding solder paste measuring equipment.

reply »

ADRIANO FERNANDES

#12070

Re: Solder Paste Measuring | 5 April, 1999

| I need help in finding solder paste measuring equipment. | Hi cuch,

I have two site where you could to find information about solder paste measuring equipment. The website are: www.cyberoptics.com and www.malcom.org I already worked with solder paste measuring equipment call LSM - II from cyberoptics; this equipment is very easy to use and you have goods measuring but it is off-line ( i think unique problem), please check outher models in the website cyberoptics or malcom.

Best regards

Adriano Fernandes

reply »

Karl Mighton

#12071

Re: Solder Paste Measuring | 5 April, 1999

| I need help in finding solder paste measuring equipment.

CHECK OUT www.isystems.com I Systems has what you need for 3d measurment. |

reply »

Dean

#12072

Re: Solder Paste Measuring | 5 April, 1999

| | I need help in finding solder paste measuring equipment. | | | Hi cuch, | | I have two site where you could to find information about solder paste measuring equipment. The website are: www.cyberoptics.com and www.malcom.org | I already worked with solder paste measuring equipment call LSM - II from cyberoptics; this equipment is very easy to use and you have goods measuring but it is off-line ( i think unique problem), please check outher models in the website cyberoptics or malcom. | | Best regards | | Adriano Fernandes | Also check out ... Orbotech Philips industrial automation

Regards, Dean

reply »

Russell Bartley

#12073

Re: Solder Paste Measuring | 5 April, 1999

| I need help in finding solder paste measuring equipment. | As already mention in other replies the Cyberoptics and others are commonly used but the price and the measurement range must be considered since you can purchase paste measurement equipment for as little as $500 (a micrometer) and up.

Russell Bartley

reply »

#12074

Re: Solder Paste Measuring | 6 April, 1999

| I need help in finding solder paste measuring equipment. | Cuch: What aspect about paste are you trying to measure?

1 Paste qualification? 2 Incoming quality? 3 Print volume?

Dave F

reply »

ScottM

#12075

Re: Solder Paste Measuring | 6 April, 1999

| I need help in finding solder paste measuring equipment. | Height, length, width, area, volume after printing (off line):

1. Cyberoptics:1-800-745-6315 www.cyberoptics.com 2. Manix Manufacturing 1-215-953-9797 3. Theta Group 1-205-650-0535 4. ASC International 1-612-416-4900

PCB Solder Paste In-line Inspection:

1. Cyberoptics (see 1. above) 2. Theta Group (see 3. above) 3. MTV Technology Ltd. 1-313-429-1712 www.mvt.ie

Viscosity of Solder Paste:

1. Stony Brook Scientific 1-201-863-2212 2. Malcom Instruments 1-510-293-0580 www.maclom.org.

Those are the ones I know of...

Good Luck, Scott

reply »

Cuch

#12076

Re: Solder Paste Measuring | 6 April, 1999

| | I need help in finding solder paste measuring equipment. | | | Cuch: What aspect about paste are you trying to measure? | | 1 Paste qualification? | 2 Incoming quality? | 3 Print volume? | | Dave F | mostly looking for print volume. I am trying to develope a fine pitch process, and would like to develop a way to inspect the paste volume before my parts get placed.

reply »

#12077

Re: Solder Paste Measuring | 7 April, 1999

| | | I need help in finding solder paste measuring equipment. | | | | | Cuch: What aspect about paste are you trying to measure? | | | | 1 Paste qualification? | | 2 Incoming quality? | | 3 Print volume? | | | | Dave F | | | mostly looking for print volume. I am trying to develope a fine pitch process, and would like to develop a way to inspect the paste volume before my parts get placed. | Cuch: Scott's listing does a good job of covering the major points, I'd like to add that some off-line measurement equipment is relatively expensive and has lousey Gauge R&R. An alternative is a microscope from:

I Systems 323 Andover St Wilmington, MA 01887 978.657.0149 Steve Pimpis www.isystems.com Start International 800.259.1986 fax 214.702.9951 Screen Manufacturing Technologies (Smart Measure Optical Z-Axis measurement system) ($1.6k) 408-562-2033 Jim Vaughn View Engineering 313.332.7600fax7799

Good luck

Dave F

reply »

Owen

#12078

Re: Solder Paste Measuring | 15 April, 1999

| I need help in finding solder paste measuring equipment. | No matter what measuremnt system you purchase, make sure that you perform a Gage R&R study to determine whcih system can meet your standards. Most manual measuremnt systems cannot adequately measure paste repeatabily. If you are looking for quality improvements, at minimal look for a semi-automated measuremnt device.

Look for a company with documented Gage R&R study imformation. If a company can't provide you with this type of information immediately, I would seriously question the systems capabilites. They should also be willing to guarentee these results in writing before you buy.

Good Luck in your search.

Owen

reply »

Owen

#12079

Re: Solder Paste Measuring | 15 April, 1999

| | I need help in finding solder paste measuring equipment. | | | No matter what measuremnt system you purchase, make sure that you perform a Gage R&R study to determine whcih system can meet your standards. Most manual measurement systems cannot adequately measure paste repeatably. If you are looking for quality improvements, at minimal look for a semi-automated measurement device. | | Look for a company with documented Gage R&R study information. If a company can't provide you with this type of information immediately, I would seriously question the systems capabilities. | They should also be willing to put these results in writing before you buy. | | Good Luck in your search. | | Owen | | |

reply »

Jade Series Selective Soldering Machines

SMT Machines china