Wave Solder Processs Control

#2562

Wave Solder Processs Control | 3 November, 2000

Has anybody done an evaluation on Wave Solder Process Control Modules? I am looking at the ECD WaveRIDER or the Wave Solder Optimizer to try and implement process control on our wave soldering operations. Which is better for controlling the process or is there something better out there.

Thanks,

reply »

#2563

Re: Wave Solder Processs Control | 3 November, 2000

Consider searching the fine SMTnet Archives

reply »

SONO-TEK CORPORATION

#2564

Re: Wave Solder Processs Control | 4 November, 2000

Mark - The Waverider is a great tool. It will let you know what's going on with the machine itself - contact time in the wave, parallelism of the wave, temp, and a relative idea of whats happening in the preheat section, and conveyor speed. We have seen many facilities that rely on these types of devices. Good luck. Claudine Sono-Tek Corporation Tel:845-795-2020

reply »

jackofalltrades

#2565

Re: Wave Solder Processs Control | 7 November, 2000

We use the Optimizer on all our waves (13) with good results.

reply »