getting boards clean | 17 August, 2000

We are using a water wash paste for our boards which is leaving ionic contamination ( salts). In the presence of low humidity levels this creates the effect of a capacitor. Our product which is test instrumentation does not calibrate. I am looking for paste and/ or process suggestions.

This message was posted via the Electronics Forum @

reply »

Travis Slaughter

#3266

Re: getting boards clean | 17 August, 2000

If your not already try DI water in your washer.