Tinlead splashes on gold connectors

RB

#31496

Tinlead splashes on gold connectors | 25 November, 2004

Something went wrong during the screening proces. So there are som tinlead splashes on the gold connectors. Can anyone give me a suggestion how to remove the tinlead splashes

reply »

#31497

Tinlead splashes on gold connectors | 25 November, 2004

Search the fine SMTnet Archives for contacts, while you await other responses.

reply »

#31530

Tinlead splashes on gold connectors | 30 November, 2004

When you say something went wrong in the screening process, do you mean that the paste is splashed (prior to reflow)?

reply »


RDR

#31532

Tinlead splashes on gold connectors | 30 November, 2004

If you are lucky, you might be able to chip the solder off the fingers with an Exacto knife and then polish it up with a pink eraser. This does work if the solder on the fingers isn't wetted very well.

Russ

reply »