I wonder if anybody could spec a conformal coating or simalar application, to protect PCB's at 90% humidity. Standard HPA from electrolube does not work if the humidity is in excess of 75%.

Cheers

reply »

#36565

Conformal coating for 90% humidity | 8 September, 2005

Try contacting Humiseal. They are BIG in conformal coating materials:

http://www.humiseal.com/

reply »

#36568

Conformal coating for 90% humidity | 8 September, 2005

Urethane CC have greater resistance to solvents than acrylic CC

reply »

#36569

Conformal coating for 90% humidity | 8 September, 2005

Slaine

#36576

Conformal coating for 90% humidity | 9 September, 2005

we use humiseal for military a customer, in an aerosol can, gives good results