Electronics Forum | Thu Sep 07 10:39:34 EDT 2006 | vicknesh28
Can u elaborate on the bad plating? Have u had any experience on this before? The component has 90/10 Tin lead plating
Electronics Forum | Fri Nov 07 15:57:56 EST 2003 | Marc Simmel
Are there specifications or recommendations for electro-deposited tin-lead plating thickness on austenitic stainless steel that would provide a shelf life of 1 year? 6 months? Would 2 to 3 microns (78 to 118 micro-inches) 90/10 tin-lead over 1.27 mi
Impact of Reflowing A Pb-free Solder Alloy Using A Tin/Lead Solder Alloy Reflow Profile On Solder Joint Integrity If you don't see images, please visit online version at #Application.SmtNet.baseURL#/express/ The Impact of Reflowing A Pb
Surface Mount Technology Association (SMTA) | https://www.smta.org/knowledge/proceedings_abstract.cfm?PROC_ID=5255
) European Union Directive has significantly reduced the use of tin/lead surface finishes for component terminations. A reexamination of solder joint wetting of lead-free solders with the new component terminations is key to establishing thermal process profiles that ensure acceptable solder joint integrity
PCB Libraries, Inc. | https://www.pcblibraries.com/Forum/RSS_library-expert-2018-09-released_topic2413.xml
2018.09 was just released!!NEW / ENHANCED:Small Outline L-Lead (SOL)Added a 10 and 12 pin versionLibrary Editor:When selecting Create New Row, the new columns “Mounting Type” and “Part Status