Electronics Forum | Tue Aug 30 09:24:08 EDT 2005 | Slaine
we manufacture a range of ceramic parts that have silver termination,there is already a small leaching problem (absorption of the termination by the solder in liquid form)with Sn62 that we live with, having to implement unleaded solder they are norma
KingFei SMT Tech | https://www.smtspare-parts.com/buy-surface_mount_parts-page2.html
: Tape Guide 2, Part Number: J7000791 3, Model: CP44mm 4, Brand: Samsung 5, Condition: New Samsung CP55 PLUG PT ... Read More Get Best Price 2022-12-20 11:26
Heller Industries Inc. | https://hellerindustries.com/wp-content/uploads/2018/07/pan_APEX06.pdf
), and the inherent strength of the solder all factor into the reliability of the solder joint. This paper presents experimental results on the effect of reflow profile on both 63%Sn 37%Pb (SnPb) and 96.5%Sn 3.0%Ag 0.5%Cu (SAC 305