Pd/Ag doesn't usually dissolve (leach) nearly as bad as Ag only. In my hybrid days, we would use 62/36/2 solder. The 2% silver helps saturate the solder joint and thus keep the Ag from being leached away by the Sn.
Electronics Forum | Wed Aug 23 16:46:52 EDT 2000 | Dr. Ning-Cheng Lee
Comparing 62Sn/36Pb/2Ag with 63Sn/37Pb, addition of 2% Ag introduces two major advantages. The first advantage is grain refining, and the resultant better fatigue resistance. The second advantage is a wider processing window on Ag metallization. Pres