ORION Industries | http://orionindustries.com/pdfs/nomex410.pdf
must be heated between 240°C and 350°C (again depending on thickness) before its LOI declines below the flammability threshold. The LOI data for Type 410 – 0.13 mm (5 mil) is shown in Figure 11. The effect of 6400 megarads (64 Mgy) of 2 MeV beta