We are facing low quality due to soldering opens with coilcraft inductors 0402CS-2N7XGLW. The termination used is(suffix L =RoHS compliant silver-palladium-platinum-glass frit. Did anyone had this problem in the past? Can we do better using T = RoH
Electronics Forum | Thu May 25 03:31:17 EDT 2006 | slaine
Hi I manufacture ceramic parts that have a terminations that are palladium/platinum/silver or any combination of the 3. Termination Ink usually consists of 3 main parts the alloy, glass frit and binder. Binder is to help bind everything together whi