ENIG poor wetting

Electronics Forum | Wed Jul 31 17:35:16 EDT 2002 | davef

* Finally, when soldered by hand, do the problem pads take solder? Yes, the XRF analysis will be interesting.

ENIG poor wetting

Electronics Forum | Mon Jul 29 16:43:55 EDT 2002 | mcm4me

I have a customer with up to 8% scrap from one board supplier and 1% from another supplier for solder dewett and no wet over ENIG finish with mask defined pads. Initially I suspected mask residue on pads because of the no wets but I have come to find

__FOOTER__

Industry News: enig poor solder flow (6)

An Analysis of SMT Solder Paste Printing Defects

Industry News | 2018-10-18 08:27:03.0

An Analysis of SMT Solder Paste Printing Defects

Flason Electronic Co.,limited

How To Set Profile In SMT Reflow Oven

Industry News | 2018-10-18 09:37:27.0

How To Set Profile In SMT Reflow Oven

Flason Electronic Co.,limited

__FOOTER__

Technical Library: enig poor solder flow (1)

Understanding the Effect of Process Changes and Flux Chemistry on Mid-Chip Solder Balling

Technical Library | 2016-11-30 21:30:50.0

Mid-chip solder balling is a defect typically associated with solder paste exhibiting poor hot slump and/or insufficient wetting during the reflow soldering process, resulting in paste flowing under the component or onto the solder resist. Once molten, this solder is compressed and forced to the side of the component, causing mid-chip solder balling.This paper documents the experimental work performed to further understand the impact on mid-chip solder balling from both the manufacturing process and the flux chemistry.

Henkel Electronic Materials

__FOOTER__

Career Center - Jobs: enig poor solder flow (2)

Assembler 2 – IPC 610 – 1st Shift

Career Center | Oldsmar, Florida USA | Engineering,Maintenance,Production

Job Title: Assembler 2 – IPC 610 – 1st Shift Address: 3655 Tampa Rd, Oldsmar FL 34677 Duration: 1 year Pay Rate: $15-$18 Hours: 9/80 schedule Monday – Thursday 6:00AM – 3:30PM, Friday 6:00AM to 2:30PM Job Description: Use microscope to verify

Lockheed Martin Corporation

Senior Assembler

Career Center | Oldsmar, Florida USA | Maintenance,Production

Job Description: • Uses microscope to verify correct part placement and orientation, manually align parts before soldering and perform post re-flow inspection and touch-up. • Able to identify and touch up poor wetted solder joints, solder voids / i

intiGrow

__FOOTER__

Express Newsletter: enig poor solder flow (1009)


enig poor solder flow searches for Companies, Equipment, Machines, Suppliers & Information