soft gold vs immersion gold

Electronics Forum | Wed Aug 11 18:36:03 EDT 2004 | davef

90 Knoop. Q2: Thickness is 4 to 10 u" for Au and 300 to 400 u" for nickel A2: This looks like a ENIG spec. Although, the Ni is quite heavy, 150 uin is sufficient for most applications. [IPC-4552 ENIG specification: * Gold thickness of 0.075 - 0.125

Re: non-wetting on gold land pad

Electronics Forum | Fri Oct 29 10:02:28 EDT 1999 | John Thorup

Chris A lot of people have reported sudden, fab lot related problems with Ni/Au pads. These are usually characterized by a discoloration of the gold and called cheerful names like "black pad disease". This can be a process problem at your fab house

Express Newsletter: gold discoloration (85)

SMTnet Express - August 7, 2014

SMTnet Express, August 7, 2014, Subscribers: 23058, Members: Companies: 13975, Users: 36604 Gold Embrittlement In Lead-Free Solder. Craig Hillman, Nathan Blattau, Joelle Arnold, Thomas Johnston, Stephanie Gulbrandsen; DfR Solutions , Julie Silk


gold discoloration searches for Companies, Equipment, Machines, Suppliers & Information

Sm t t t t t t t t t t net
  1 2 3 4 5 6 7 8 9 10 Next